Which of the following is an example of stress corrosion ?
Correct answer: D. Both A. & B.
- A. Season cracking of brass
- B. Caustic embrittlement of steel
- C. Neither A. nor (B)
- D. Both A. & B.
Explanation
Season cracking of brass and caustic embrittlement of steel are both forms of stress-corrosion failure, requiring a susceptible metal, a corrosive environment and tensile stress. Thus, both listed examples qualify.
Report an error
The more specific you are, the faster it gets fixed. A source beats an opinion.
Prefer email? [email protected]
Practise Chemical Process Principles
2,710 free Chemical Process Principles MCQs from Chemical Engineering, each with the correct answer and an explanation. Unlimited attempts, no account needed.
Discussion
Stuck on an option, or know a faster way to get there? Ask or explain it here.
No comments yet. Be the first to explain this one.
Exams that ask Chemical Engineering questions like this
Chemical Engineering is on this paper prepared for on TestUstad, and all of them draw the same bank, so this question is worth knowing for it.
More Chemical Process Principles questions
Drills are usually made of__________________?
Silicon crystal can be converted to p-type semi-conductor by doping with__________________?
Tesla metre per ampere (T. m/A) is the unit for the measurement of_______________?
Silicon percentage in the silicon steel used for electrical appliances/equipments is_________________?
Catalyst used in the 'catalytic converter' employed in automobile exhaust line for complete combustion/oxidation of carbon monoxide, nitrogen oxides and hydrocarbons is__________________?
Annealing of cast iron__________________?