When concrete is remixed after partial loss of workability, the most appropriate correction is generally to

Correct answer: C. Remix it without adding water unless the specification permits adjustment

  • A. Add dry coarse aggregate without changing other ingredients
  • B. Add water freely until the original slump is restored
  • C. Remix it without adding water unless the specification permits adjustment
  • D. Allow it to set and then compact it by heavy vibration

Explanation

Remixing may restore uniformity, but adding unapproved water raises the water-cement ratio and can reduce strength and durability. Any permitted adjustment must follow the approved mix procedure, not be made freely at site.

Written and checked by , MS Computer ScienceLast updated
Report an error

The more specific you are, the faster it gets fixed. A source beats an opinion.

Prefer email? support@testustad.com

About Concrete Technology

Concrete technology covers cement, aggregates, water and admixtures, including their properties, proportioning and effect on fresh and hardened concrete. It explains workability, water-cement ratio, setting, hydration, strength, durability, curing, mix design and common defects, while distinguishing segregation and bleeding from general loss of workability.

Practise Concrete Technology

80 free Concrete Technology MCQs from Civil Engineering, each with the correct answer and an explanation. Unlimited attempts, no account needed.

Discussion

Stuck on an option, or know a faster way to get there? Ask or explain it here.

No comments yet. Be the first to explain this one.

Exams that ask Civil Engineering questions like this

Civil Engineering is on 3 papers prepared for on TestUstad, and all of them draw the same bank, so this question is worth knowing for every one of them.

More Concrete Technology questions