Subsurface porosity is due to_____________?
Correct answer: A. Thermal changes
- A. Thermal changes
- B. Thickness of the resin
- C. Lack of temperature
- D. Packing past the dough stage
Explanation
Subsurface porosity in acrylic resin commonly results from overheating, which vaporizes monomer within the resin mass; the risk rises in thick sections. Packing beyond the dough stage mainly causes poor adaptation or other packing defects rather than being the principal cause here.
Report an error
The more specific you are, the faster it gets fixed. A source beats an opinion.
Prefer email? support@testustad.com
Practise Polymers in Dentistry
39 free Polymers in Dentistry MCQs from Dental Materials, each with the correct answer and an explanation. Unlimited attempts, no account needed.
Exams that ask Dental Materials questions like this
Dental Materials is on this paper prepared for on TestUstad, and all of them draw the same bank, so this question is worth knowing for it.
More Polymers in Dentistry questions
Denture acrylics contain cross-linking agents mainly to improve their_____________?
The process wherein two or more chemically different monomers, each with some desirable property, can be combined to yield specific physical properties of a polymer is known as_____________?
The accepted polymer to monomer ratio for packing of polymethyl methacrylate resin is____________?
If resin is packed in sandy stage what will be seen in the processed denture ?
Insufficient closure of the flasks during packing of denture base resin can result in_____________?
Polymerisation of heat-cured methyl methacrylate is initiated by______________?