If curing occurs at temperature more than 100°C porosity results in which area of denture______________?

Correct answer: D. Hard thick central area

  • A. Porosity is uniformly distributed
  • B. Thin Palatal area
  • C. Thin area of flanges
  • D. Hard thick central area

Explanation

Heating denture acrylic above the boiling point of its monomer produces gaseous monomer porosity, especially in the thick central portion where heat is retained. Thin areas allow heat and monomer vapour to escape more readily.

Submitted by a TestUstad contributor and published by the TestUstad editorial teamLast updated
Report an error

The more specific you are, the faster it gets fixed. A source beats an opinion.

Prefer email? [email protected]

Practise Polymers in Dentistry

39 free Polymers in Dentistry MCQs from Dental Materials, each with the correct answer and an explanation. Unlimited attempts, no account needed.

Discussion

Stuck on an option, or know a faster way to get there? Ask or explain it here.

No comments yet. Be the first to explain this one.

Exams that ask Dental Materials questions like this

Dental Materials is on this paper prepared for on TestUstad, and all of them draw the same bank, so this question is worth knowing for it.

More Polymers in Dentistry questions