Identify the false statement?
Correct answer: A. Martensitic steels are less susceptible to pitting corrosion than austenitic steels
- A. Martensitic steels are less susceptible to pitting corrosion than austenitic steels
- B. Pitting corrosion is usually very localised
- C. Hydrogen embrittlement is facilitated by tensile stress
- D. Stress corrosion cracking is facilitated by tensile stress
Explanation
Martensitic stainless steels generally have lower corrosion resistance and are more prone to pitting than austenitic stainless steels, so statement a is false. Pitting, hydrogen embrittlement, and stress-corrosion cracking are correctly associated with the behaviours stated in b, c, and d.
Report an error
The more specific you are, the faster it gets fixed. A source beats an opinion.
Prefer email? support@testustad.com
Practise Chemical Process Principles
2,710 free Chemical Process Principles MCQs from Chemical Engineering, each with the correct answer and an explanation. Unlimited attempts, no account needed.
Exams that ask Chemical Engineering questions like this
Chemical Engineering is on this paper prepared for on TestUstad, and all of them draw the same bank, so this question is worth knowing for it.
More Chemical Process Principles questions
What happens, when SO2 is passed through a solution of H2S in water ?
Specific gravity of hot metal (pig iron) is ______________ times that of the blast furnace slag ?
Which of the following pairs is not correctly matched ?
Steels with high carbon equivalent have poor Weldability, because in these steels during welding________________?
Blasting of tri-nitro-toluene (TNT) is done by mixing it with ammonium_______________?
_________________ property of a material is determined by the Herbert Pendulum device?