Faster rate of drying of moulded refractories results in high _____________ of refractories?
Correct answer: D. Both B. and C.
- A. Green strength
- B. Voids
- C. Shrinkage
- D. Both B. and C.
Explanation
Rapid drying can produce nonuniform moisture removal, causing greater shrinkage and internal voids or cracks in the moulded refractory. Hence both voids and shrinkage increase.
Report an error
The more specific you are, the faster it gets fixed. A source beats an opinion.
Prefer email? support@testustad.com
Practise Plant Design and Economics
803 free Plant Design and Economics MCQs from Chemical Engineering, each with the correct answer and an explanation. Unlimited attempts, no account needed.
Exams that ask Chemical Engineering questions like this
Chemical Engineering is on this paper prepared for on TestUstad, and all of them draw the same bank, so this question is worth knowing for it.
More Plant Design and Economics questions
Silica refractories are not used in _________________?
Porosity of silica bricks varies from ______________ percent?
Alumina-graphite bricks are used for lining the ____________________?
Roof of a basic electric furnace is made of _____________ bricks?
Outer combustion chamber of blast furnace stove is lined with _____________ bricks?
Magnesite refractories are used for the construction of those furnaces, which are________________?